John, I assume you are talking about double side PCB but not multilayer. If you see that the resin is very smoothly separated from the fiber, it’s the wetting of the resin to the glass fiber issue. If it’s crack on the resin, it may be the resin is not fully cured or the laminate is make from expired PP…….. If possible, attached a x-section photo for me to see. With Best Regards Joseph Ho --------------------------------- Senior Manager Customer Quality Management Tel: (86) 756 5329308 MP: (86) 13825650969 Creating value that increases customer competitiveness ________________________________ From: TGAsia [mailto:[log in to unmask]] On Behalf Of John Zhou Sent: Monday, August 23, 2010 11:54 AM To: [log in to unmask] Subject: Re: [TGAsia] PCB 分层问题 各位大虾: 请教个PCB分层问题, 我们的PCB 在过IR reflow 之后约有0.5%-1%的分层问题,可以排除潮湿问题(PTH前有烤155度,4小时,24小时内完成PTH), PCB工艺完成之后马上到EMS工厂组装,看切片也不象压合的问题,因为都是PP片内部分层而不是层与层之间分开. 目前我们怀疑PP有问题, 但是RC.RF, Gel time 和 VC 值都在规格内, 正在准备测试260分层时间和热裂解温度和PP的桥接剂dicy的再结晶,诸位大虾知道哪里可以检查PP材料里面的桥接剂dicy再结晶?PP还有什么需要测试的吗? John Zhou/Supplier Quality Engineer Pace China MP#: (0086) 138 2528 2354 深圳宝安机场进场大道机场信息大楼六层东区646-648室 Rm 646-648 F/6, East, ShenZhen Airport Information building, Airport Entrance road, BaoAn District, ShenZhen, 518218 This message has been scanned for viruses by BlackSpider MailControl <http://www.blackspider.com/> ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please visit http://www.messagelabs.com/email ______________________________________________________________________ ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ Legal Disclaimer: The information contained in this message may be privileged and confidential. It is intended to be read only by the individual or entity to whom it is addressed or by their designee. If the reader of this message is not the intended recipient, you are on notice that any distribution of this message, in any form, is strictly prohibited. If you have received this message in error, please immediately notify the sender and delete or destroy any copy of this message ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________