Years ago I was doing plasma deposition of a variety of hydrocarbons. I cleaned with argon plasma, then wiped out chamber to remove bulk deposits, then cleaned with oxygen plasma. It was a lab environment. Each of the cleaning cycles was about an hour. Dick Krug, CSMTPE SMT Process Engineer Sparton Corporation 30167 Power Line Road Brooksville, FL 34602-8299 p (352) 540-4012 (Internal Ext. 2012) [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls Sent: Friday, July 30, 2010 9:01 AM To: [log in to unmask] Subject: [TN] Plasma Chamber Maintenance Good morning all, On a topic other than rhubarb, raiding my cubicle for prizes, and selling off my children, I have an actual technical question. We have started to use plasma chambers as a preparation for conformal coating and are having some excellent results. One of our IEs, with a background in the semiconductor industry, had indicated that the chambers can be items that are hard to maintain or high in maintenance costs. So, for you plasma chamber users out there, what have your experiences been with plasma chamber maintenance? Doug Pauls ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------