I don't think you'll have a problem with that amount of Ni. Vladimir SENTEC Testing Laboratory Inc. 11 Canadian Road, Unit 7. Scarborough, ON M1R 5G1 Tel: (416) 899-1882 Fax: (905) 882-8812 www.sentec.ca -----Original Message----- From: David R1 Nelson <[log in to unmask]> Sender: TechNet <[log in to unmask]> Date: Wed, 7 Jul 2010 14:58:56 To: <[log in to unmask]> Reply-To: TechNet E-Mail Forum <[log in to unmask]>, David R1 Nelson <[log in to unmask]> Subject: [TN] Ni in Eutectic SnPb solder We have come upon a situation where the trace element Ni is above the J-STD-001D threshold for an assembly wave solder machine with a reading of 0.015% to 0.020%. I'd like to know if anyone has experience or knows of any studies done to determine the impact of this higher limit on the products produced using this equipment. All advice/references would be appreciated. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________