However, making the pad small may affect the paste release from the stencil, especially as the board may not be very accurate and the board to stencil alignment may not always be perfect. Given all those maybe-s, the pad has to "suck" (technical term) the paste out of the stencil and only the aligned portion of the pad does the best "sucking". Having fun, Ahne. PS: does anybody have a spec on the precision of the board image? (????????) -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier Sent: Thursday, July 08, 2010 10:20 To: [log in to unmask] Subject: Re: [TN] 0201 footprint requirements Hi Bill, Little or no extension beyond cap outline-both lengthwise and in the width. Werner -----Original Message----- From: Brooks, Bill <[log in to unmask]> To: [log in to unmask] Sent: Thu, Jul 8, 2010 1:09 pm Subject: Re: [TN] 0201 footprint requirements I see, So... what size should the land pattern be for a 0201 cap? Bill Brooks | Datron World Communications, Inc. PCB Designer/Engineer | Office: 760-602-7004| Fax: 760-597-3777 | [log in to unmask] 1808 Aston Avenue, Suite 230, Carlsbad, CA 92008 | www.dtwc.com Performance You Require. Value You ExpectTM -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier Sent: Wednesday, July 07, 2010 7:36 PM To: [log in to unmask] Subject: Re: [TN] 0201 footprint requirements Hi Bill, Indeed, larger footprints are a recipe for not only tombstoning, but component cracking as well. Werner ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------