Hi Inge- No, no requirement for "half moon crescent", other than, if you have good pulltest data, the flameoff process is working well, and the underlying pad you are stitching to isn't damaged, then probably you will have a nice crescent. No, never used Manson. We encapsulate or overmold everything we make, so vibration isn't an issue. And if repetitive thermal cycles are the problem, then I suspect that the intermetallic areas are more likely going to fail first. As a matter of fact, once predicted failures go out more than 20 years, a whole bunch of low probability of occurrence stuff has a chance to happen! Was the stress you analyzed due to vibration? You mention Kovar and alumina, but I thought those were supposed to be matched closely enough that rates of thermal rise and thermal conductivity are more important than linear coeff of elongation. Wayne -----Original Message----- From: Inge [mailto:[log in to unmask]] Sent: Wednesday, June 16, 2010 4:54 PM To: Thayer, Wayne - IIW; [log in to unmask] Subject: Re: [TN] ? Thanks Wayne. 1. No aspect on 'half moon crescent' ? 2. Have you or someone else practised Manson's universal slope equation for calculation of life expectancy of bond wires? Delta epsilon = 3.5 x sigma b/E x Nf exp-0.12 + epsilon1 exp 0.6 x Nf exp -0.6 where Delta epsilon = elongation sigma b = rupture tension E = elasticity module Nf = number of cycles to rupture epsilon1= rupture elongation We used this for deciding how many cycles gold wires would withstand in a typical MIL aircraft application when the substrates were alumina and the packages Kovar. The result was som 50,000 - 100,000 cycles or 60-120 years for -55/+125C. The question is how much one can rely on this calculation model. Anyone done similar ? Personally I thing one should only see such calculations as estimations only. Inge -------------------------------------------------- From: "Thayer, Wayne - IIW" <[log in to unmask]> Sent: den 16 June 2010 20:57 To: <[log in to unmask]> Subject: Re: [TN] ? > Hi Inge! > > 5 grams per square mil average shear for gold ball bonding > Avg - 3 x StdDev > 3 grams for 1 mil gold destructive pull test > > The latter is kind of vague because the wire set must be large enough to > get a good sample size and all of the loops have to have reasonable > heights and must be similar. > > For aluminum, we're very application-dependent, but use the Avg - 3 x > StdDev as the parameter of interest. > > These don't test how close to cratering we are, which is an industry-wide > issue. > > Visually, we are looking for a consistent rim on the ball, and a rim > height no greater than about one half of the wire diameter. For the > stitch, consistency and virtually no capillary imprint from the stitch > process on the lead/land. > > Wayne > > -----Original Message----- > From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge > Sent: Wednesday, June 16, 2010 1:58 PM > To: [log in to unmask] > Subject: [TN] ? > > What standards do you use for inspection and qualification of wire bonding > today? > Thanks > IInge > > > ______________________________________________________________________ > This email has been scanned by the MessageLabs Email Security System. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- > > This e-mail and any files transmitted with it may be proprietary and are > intended solely for the use of the individual or entity to whom they are > addressed. If you have received this e-mail in error please notify the > sender. > Please note that any views or opinions presented in this e-mail are solely > those of the author and do not necessarily represent those of ITT > Corporation. The recipient should check this e-mail and any attachments > for the presence of viruses. ITT accepts no liability for any damage > caused by any virus transmitted by this e-mail. > > ______________________________________________________________________ > This email has been scanned by the MessageLabs Email Security System. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------