Dear All, I have 3 queries in all..... 1. One of our customer has changed the surface finish from HASL to ENIG. Their main reason for this change was that they have had a bad experience with storage of HASL finished boards (the reason for which is not shared with us). They had encountered solderability problems on the HASL finished board which they had stored for a period of time. Their expectation with Gold plated surface is the storage of the PCBs can be for a longer period of time as compared to HASL finish. Initially they had a requirement for 1micron thick electrolytic gold, but later on they changed the requirement for an ENIG process with gold around 0.05 to 0.10 microns. Now my question...... Is there any guideline on the shelf life of the PCBs (with regard to solderability) of the following surface finishes.... a) ENIG b) HASL c) Immersion Tin d) Electrolytic Ni and electrolytic gold with Gold thickness of 1.0microns Will vacuum packing help to extend the shelf life? 2. One of our customer is doing hand soldering of PCBs with ENIG finish. They're inserting a strand of tinned Copper wires from component side and later on using soldering iron to do the soldering from the solder side. The solder is able to flow up from solder side to component side, but the solder is unable to complete wet the pad on the component side. I've attached the photos of example of the phenomenon. These photos are without the wire, I've just used bare PCBs to do the soldering to illustrate the phenomenon. Now my question.... a) Will increasing the volume of the solder help in complete wetting of the pads on the component side? b) Any other way to get a full coverage on the pads on the component side. 3. This question is about the same customer which I've mentioned in para 2 above, is doing hand soldering. In one of the stage of component assembly, they're (hand) soldering a flexible PCB on the ENIG finished rigid PCBs. They have a unique practice during this stage of soldering. They've explained to us that this particular component is very sensitive to high temperature and hence the soldering iron temperature is set at 210Deg C. They're using Sn60/Pb40 solder for this soldering operation. After the soldering iron achieves 210Deg C, they're turning off the power to the soldering iron and doing the soldering of the flexi PCB onto the rigi PCBs. We'll not know the actual soldering iron temperature at the point of contact. They've complained to us that the soldering is poor. We know that the melting temperature of solder is around 183deg C. But, is there any guideline on the minimum temperature for soldering to get a good flow of solder and completely wetted solder? Thanks for your inputs in advance. Best Regards, U.Nagaraj MICROPACK Ltd, Bangalore, INDIA. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------