We have an old copy of an Excel stack-up model from Isola. It says that for a 1080 pre-preg with 65% resin that you need about 80% copper on two adjacent 1oz copper layers to ensure sufficient resin fill. While the model provides only a guide I would certainly be concerned about the scenario that you are describing and would not recommend it to any of our customers. Good luck, John Parsons -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Frank Kimmey Sent: Tuesday, June 01, 2010 8:46 AM To: [log in to unmask] Subject: Re: [TN] Single-ply construction Dan, From a Designer's view I can see serious issues here. Firstly there will be a huge risk of delam due to poor fill at traces (you will need to fill 2.4 mill minimum at trace and pad locations) Then there is the issue of dielectric isolation between layers (only about 2 mils with one layer 1080) Then probably some capacitive issues due to proximity of copper to signal (SI problems) I would suggest some further discussion with your customer and possibly listing for them your concerns, then build what they ask for and try not to say "I told you so" Or tell them you cannot guarantee the construction and no-bid to save them the bad lesson they are risking Good luck, FNK Frank N Kimmey CID+ Manager - PCB Design Powerwave Technologies Inc Mobile - 916-670-0645 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Dan Skweres Sent: Tuesday, June 01, 2010 8:20 AM To: [log in to unmask] Subject: [TN] Single-ply construction We have a customer insisting that we use a single ply of FR406 1080 between two copper layers each 1 oz. copper. One layer is a plane and the other a signal. We're quite concerned that there will be issues with fill. We don't recommend single-ply construction especially against two 1 oz. copper layers. Any thoughts, comments and/or concerns would be appreciated. Thanks! Dan S. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------