Hi Grant, any METAL case will work. What you create is a Faraday cage, that will eliminate electrostatic and electromagnetic influence. However, it will NOT eliminate static magnetic fields, nor low frequency electromagnetic waves. In such a case you'll need ferro materials, one of the best being so called mu metal. But, as your question was about RF, pewter will work, not as good as ferro materials, but it depends on the pewter wall thickness. In many modern electronics, you get acceptable RF shielding by means of plastic boxes with a thin metal coating only. Works for weak RF signals, which are often the case within commercial products like mobile telephones and transistor radios. Speaking RF signals at radar levels, magnetrons, klystrons, TWTs and other high power sources, I would not use pewter. Inge -------------------------------------------------- From: "Grant Emandien" <[log in to unmask]> Sent: den 9 June 2010 11:22 To: <[log in to unmask]> Subject: [TN] Pewter as RF screening material > Hi, > > Does anyone used lead-free pewter for RF screening purposes? > > Pros & Cons? > > Regards > Grant > > ______________________________________________________________________ > This email has been scanned by the MessageLabs Email Security System. > For more information please contact helpdesk at x2960 or [log in to unmask] > ______________________________________________________________________ > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------