Hi Torsten Henkel Macromelt encapsulation might be worth a look. http://www.henkel.com/adhesives/MA_Macromelt_Homepage-12494.htm - no personal experience with it but it is an interesting process. regards, - Graham -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Torsten Hagge Sent: Tuesday, May 25, 2010 7:31 AM To: [log in to unmask] Subject: [TN] Coating Hi Technetters, looking for an conformal coating for electronics used in medical application. The small electronic should be able to pass 1000 cycles washing and cleaning process with ph=13 plus 20 minutes autoclave 135°C @ 2bar. 1st idea is parylene coating, any cheaper or better ideas? Regards, Torsten Dipl.Ing.(FH)Torsten Hagge tech. projectmanager Kristronics GmbH Gewerbegrund 5 - 9 24955 Harrislee Tel.: +49 461 7741 624 Fax: +49 461 7741 642 [log in to unmask] www.kristronics.de Gerichtsstand Flensburg, Handelsregister: HRB 1433 FL Geschäftsführer Dipl.-Ing. oec. Thormod Ohm Ust-Id-Nr. DE 811182059 Bankverbindung: Deutsche Bank AG Flensburg, Konto-Nr. 4216610, BLZ 21570011 IBAN: DE32 2157 0011 0421 6610 00, BIC: DEUT DE HH 215 ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------