Ioan, FYI, depending on the extent of cold work, austenitic stainless can exhibit a degree of magnetism, albeit weak. Regards Ian -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea Sent: 21 May 2010 20:57 To: [log in to unmask] Subject: Re: [TN] RoHS compliance of stainless stell Rudy, You are close, it's Austenitic and Martensitic. But are they non-conditionally RoHS compliant? Looks like we have to specify, or check our customers did, 300 series, in order to validate with the magnet... sounds like a plan. Thanks, Ioan Tempea, ing. Ingénieur Principal de Fabrication / Senior Manufacturing Engineer T | 450.967.7100 ext.244 E | [log in to unmask] W | www.digico.cc N'imprimer que si nécessaire - Print only if you must -----Message d'origine----- De : R Sedlak [mailto:[log in to unmask]] Envoyé : May-21-10 3:31 PM À : [log in to unmask] Objet : Re: [TN] RoHS compliance of stainless stell Ioan: Typically, 300 series steel, which I think is called Austinetic (spelling is probably wrong) is not magnetic, and is much more corrosion resistant. Type 400 series SS, which I believe is referred to as Martinistic, is a much cheaper grade, and much more prone to corrosion, and is magnetic. Rudy Sedlak RD Chemical Company --- On Fri, 5/21/10, Ioan Tempea <[log in to unmask]> wrote: From: Ioan Tempea <[log in to unmask]> Subject: [TN] RoHS compliance of stainless stell To: [log in to unmask] Date: Friday, May 21, 2010, 6:44 AM Hi group, A rookie sort of question : can Stainless Steel be blindly considered RoHS compliant? Otherwise said, is there any SS hardware that could have any of the buggers (mainly Cd or Cr6)? Also, could some SS fall under the Pb exemption for machining? And finally, some SS alloys are magnetic, some other aren't. Can SS hardware used in our industry be magnetic? As you already guessed it, what I am trying to figure out is if I can make an incoming selection based on magnets. If non-magnetic = accept, if magnetic = reject. Thanks, Ioan Tempea, ing. Ingénieur Principal de Fabrication / Senior Manufacturing Engineer T | 450.967.7100 ext.244 E | [log in to unmask] <mailto:[log in to unmask]> W | www.digico.cc <http://www.digico.cc/> N'imprimer que si nécessaire - Print only if you must ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- -------------------------------------------------------------------------- This message (and any attachment) is confidential and is intended for the named recipient only. If you receive it in error please e-mail back the sender and permanently delete the original message and any copies. Rolls-Royce Goodrich Engine Control Systems Limited. Registered Office: Moor Lane, PO Box 31, Derby, DE24 8BJ. Registered in England No. 06686268. -------------------------------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------