Robert, for Flat Ribbon, L, and Gull Wing Leads the sides and toe don't have to be soldered. Background as far as I know is, that these sides might not be wetable. In contrast, a wetting of one side is required for Round or Flattened Leads (8.2.6.8), because they are wettable. Frank Von: Robert N <[log in to unmask]> An: [log in to unmask] Datum: 18.05.2010 21:17 Betreff: [TN] Acceptabe Solder Fillet on Gull wings Gesendet von: TechNet <[log in to unmask]> IPC 610 Cl 2 states that a side overhang of 50% is acceptable. Does that means, which seems obvious but not stated, that an acceptable solder fillet is required on one side only? Does the same apply to the toe, which allows for an overhang? --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- . Der Inhalt dieser E-Mail ist für den Absender rechtlich nicht verbindlich. Informieren Sie uns bitte, wenn Sie diese E-Mail fälschlicherweise erhalten haben (Fax: +49-7551-891-4001). Bitte löschen Sie in diesem Fall die Nachricht. Jede Form der weiteren Benutzung ist untersagt. . The content of this e-mail is not legally binding upon the sender. If this e-mail was transmitted to you by error, then please inform us accordingly (Fax: +49-7551-891-4001). In such case you are requested to erase the message. Any use of such e-mail message is strictly prohibited. ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________