Hi gang! Here is the Friday Element Quiz answer -sorry for not getting this out but I left early on Friday to go whitewater kayaking in Wisconsin (and it snowed!). The Question: The existence of this element was predicted in 1870 and was then first isolated 5 years later. This element had no significant commercial use until 1970 and 98% of this element's production is used for a specific functionality. This element contracts approximately 3.4% upon melting. It has a very unusual crystal structure - oC8. Who am I? The Answer: I am the element Ga - Gallium Drew Meyer was first with the correct answer! And Inge is correct, I'll need to make the quiz tougher as everyone is getting the answers very quickly. Dave Hillman Rockwell Collins [log in to unmask] ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------