Bev No they don't Best regards Guenter >-----Ursprüngliche Nachricht----- >Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Bev Christian >Gesendet: Dienstag, 20. April 2010 15:16 >An: [log in to unmask] >Betreff: [TN] SAC Shrinkage Voids in BGA Balls > >TechNetters, >Do all SAC shrinkage voids in BGA balls reach/start at the surface of >the ball? I realize I may be stumped by a 2D cross-section of a 3D >phenomenon, but I thought I would ask this august body. >Bev >RIM > >--------------------------------------------------------------------- >This transmission (including any attachments) may contain confidential >information, privileged material (including material protected by the >solicitor-client or other applicable privileges), or constitute non- >public information. Any use of this information by anyone other than the >intended recipient is prohibited. If you have received this transmission >in error, please immediately reply to the sender and delete this >information from your system. Use, dissemination, distribution, or >reproduction of this transmission by unintended recipients is not >authorized and may be unlawful. > >______________________________________________________________________ >This email has been scanned by the MessageLabs Email Security System. >For more information please contact helpdesk at x2960 or >[log in to unmask] >______________________________________________________________________ > >--------------------------------------------------- >Technet Mail List provided as a service by IPC using LISTSERV 15.0 >To unsubscribe, send a message to [log in to unmask] with following text >in >the BODY (NOT the subject field): SIGNOFF Technet >To temporarily halt or (re-start) delivery of Technet send e-mail to >[log in to unmask]: SET Technet NOMAIL or (MAIL) >To receive ONE mailing per day of all the posts: send e-mail to >[log in to unmask]: SET Technet Digest >Search the archives of previous posts at: >http://listserv.ipc.org/archives >Please visit IPC web site >http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional >information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 >ext.2815 >----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------