CAF: conductive anodic filament: 离子迁移/阳极丝传导试验
CAF 的发生,将使导体间的绝缘性能下降,严重时引起电路功能失效,电路短路,严重影响产品的可靠性。
Best regards and
thanks
Nancy Deng
From: TGAsia
[mailto:[log in to unmask]] On Behalf Of 孙该贤
Sent: 2010年3月16日 9:12
To: [log in to unmask]
Subject: [TGAsia] CAF testing
请教大家一个问题,什么是CAF testing?
Sunny Sun
Quality Dept
Amphenol
Guangzhou
Amphenol Sincere Flex Circuits
Tel: 86-20-3483-9838
Fax:
86-20-3483-9800
Mobil:
13798074592
Email:
[log in to unmask]
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________