Hi,All: In IPC 7721 and 7711 document just mentioned the hot air temperature is approximately 425¡æ and adjust it if necessary £¬but it didn¡¯t define the test method to get the real temperature. Do you have the relative solutions? Thanks, Lewis Liu (Áõ¶¨ºÀ£© Engineering Department Failure Analysis laboratory Supervisor Tel:+86 -25- 52728710 Cell:+86 -25 -13851527451 Mail: [log in to unmask]<mailto:[log in to unmask]> Kimball Electronics (Nanjing) Co.,Ltd ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________