I think you can use a thomermal couple to verify the actual temperature.

Hot air temp 425 C is too high for the some components repair. You should check whether the component can bear such high temp, or not.


Thanks and best regards
Eddie



Lewis Liu <[log in to unmask]>
Sent by: TGAsia <[log in to unmask]>

03/02/2010 12:03 PM
Please respond to
Asia Committe Task Group Forum <[log in to unmask]>; Please respond to
Lewis Liu <[log in to unmask]>

To
[log in to unmask]
cc
Subject
[RMX:##] [TGAsia] measure the hot air temperature method





Hi,All:
In IPC 7721 and 7711 document just mentioned the hot air temperature  is approximately 425¡æ and adjust it if necessary £¬but it didn¡¯t define the test method to get the real  temperature.
Do you have the relative solutions?
Thanks,
 
Lewis Liu (Áõ¶¨ºÀ£©
Engineering Department  
Failure Analysis laboratory Supervisor
Tel:+86 -25- 52728710
Cell:+86 -25 -13851527451
Mail:  [log in to unmask]
Kimball Electronics (Nanjing) Co.,Ltd
 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________