Gregg, About 15 years ago at another job we returned a shipment of LCD display assemblies because their individual pink poly bags caused crazing on the plastic faces. The LCD plastic and the poly bag's ingredients were incompatible, so the vendor changed over to generic metallized ESD bags afterward. Bruce Tostevin Benchmark Electronics -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Gregg Owens Sent: Tuesday, March 30, 2010 10:04 AM To: [log in to unmask] Subject: [TN] ESD Cap Plugs Dear TechNet: There has been discussion on the use of "pink poly" for ESD prevention on flight hardware. An expressed concern has been the chemicals added to the surface of pink poly can potentially contaminate our products with the residue pink poly leaves behind. I have posted a picture of one of our boxes which have both the pink poly and black ESD style of cap plugs. What are any of your experiences with contamination associated with using pink poly? As always, thanks, Gregg Owens Technical Writer - Avionics Space Exploration Technologies Corporation 1 Rocket Road | Hawthorne | CA | 90250 310-363-6533 | [log in to unmask] ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------