Hi Graham I am looking for info on what is available to make recommendations to clients. It is becoming more and more clear, that in order to avoid a manner of problems caused by Pb-free soldering temperatures, the best option is to solder with the lowest possible temperature, and that means using vapor phase. Werner -----Original Message----- From: Graham Naisbitt <[log in to unmask]> To: TechNet E-Mail Forum <[log in to unmask]>; Werner Engelmaier <[log in to unmask]> Sent: Fri, Feb 5, 2010 5:45 pm Subject: Re: [TN] Vapor Phase soldering Hi Werner Can you be more specific? The best VP system that I know, is now available from REHM and based upon the patents of J-P Garridel (France). This employs a discontinuous conveyorised system that minimises solvent losses. Might this be what you are seeking information about? Regards Graham Naisbitt - KBO Email: [log in to unmask] Phone: +44 (0)12 5252 1500 Web: www.gen3systems.com On 5 Feb 2010, at 08:48, Werner Engelmaier wrote: > Hi All, > I would appreciate any feedback on the new vapor phase soldering ovens that have recently become available. > Werner > > > > > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------