LOL. We need more of these kind of postings on Monday mornings. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls Sent: Monday, February 01, 2010 9:00 AM To: [log in to unmask] Subject: Re: [TN] IPC-5702 / IPC-5704 Having written most of both, let me give it a shot. 5704 gives you recommended cleanliness requirements for bare/unpopulated printed circuit boards as measured by ion chromatography. It essentially duplicates Delphi's C-7000 cleanliness specification that has worked well for over a decade. It does not claim that if your boards meet these levels that they will be good for all processes, all applications, all end environments, for ever and ever, Amen. But, it is a darn good place to start until your own testing tells you better. Certainly a vast improvement over ROSE. 5702 was written to give guidance to OEMs guidance on determining how clean boards and assemblies need to be for their applications. Meant more for general education. Both brilliantly written. Must now type one handed as I have dislocated my shoulder patting myself on the back. In reality, both documents were significantly improved through the inputs of the 5-32c and 5-32a IPC working groups. Doug Pauls Rockwell Collins Delusional Engineer "Glidden, Kevin" <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 02/01/2010 08:51 AM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to "Glidden, Kevin" <[log in to unmask]> To [log in to unmask] cc Subject [TN] IPC-5702 / IPC-5704 Happy Monday everyone..... Can anyone comment on how the newly released IPC-5704 ""Cleanliness Requirements for Unpopulated Printed Boards" and the 2007 release of IPC-5702 "Guidelines for OEMs in Determining Acceptable Levels of Cleanliness of Unpopulated Printed Boards" are meant to work together? I've not yet read the new 5704, so this is just a general inquiry...... Thanks! Kevin --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------