-----Original Message----- From: Mike Sewell [mailto:[log in to unmask]] Sent: Thursday, February 11, 2010 1:56 PM To: Bob Landman Subject: RE: [TN] Old reference for silver solder - what's it cross ref to? How about 94 Lead Tin Silver for the composition? Sn05Pb93.5Ag1.5 wire solder in an activated rosin or resin with a 3.3% flux core? Alpha lists the alloy on their chart. Maybe rev E of QQ-S-571 (1972) identifies it. Mike -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Landman Sent: Thursday, February 11, 2010 12:42 PM To: [log in to unmask] Subject: Re: [TN] Old reference for silver solder - what's it cross ref to? Tektronix used a silver bearing solder for their vacuum tube oscilloscopes. The terminal strips that held the components were ceramic and they had metal slots in them to lay the component wires. It was an elegant solution. Standard 60/40 solder's coeficient of expansion would crack the ceramic so inside every scope back by the power supply was a small plastic spool of silver bearing solder. Not "silver solder" like you use to join pieces of metal, but soft pliable solder that has silver in it. I think this is what you are looking for Rudy. Not "silver solder" which takes a gas torch to melt. Bob Landman H&L Instruments (former Tek Field Engineer :-) -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak Sent: Thursday, February 11, 2010 12:54 PM To: [log in to unmask] Subject: Re: [TN] Old reference for silver solder - what's it cross ref to? Graham: This is from Wikipedia: "Silver solder is also used in manufacturing to join metal parts that cannot be welded. The alloys used for these purposes contain a high proportion of silver (up to 40%), and may also contain cadmium." Believe it or not, hand made steel frame racing bicycles were often silver soldered, as you don't need to heat the metal as hot, as when you braze. And the bond is STRONG. Rudy Sedlak --- On Thu, 2/11/10, Graham Collins <[log in to unmask]> wrote: From: Graham Collins <[log in to unmask]> Subject: [TN] Old reference for silver solder - what's it cross ref to? To: [log in to unmask] Date: Thursday, February 11, 2010, 9:42 AM Hello Technet I seem plagued with strange solder questions these days. Can somebody help with a cross-reference from an old solder callout to what this would be referred to as now? I have a drawing that references: "QQ-S-571 alloy 94LTS Type WRAP3", and refers to it as "silver solder". I can get the last version of QQ-S-571 (rev F, before it was cancelled and J-STD-006 adopted), but I do not see this type of callout. Does anyone have something that will tell me what's in this solder? Thanks! Graham Collins Halifax Production Engineering L-3 Communications ES ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------