I bet you won't see anything with C-SAM on the virgin (prior to mounting) dice :-) Vladimir SENTEC 11 Canadian Road, Unit 7. Scarborough, ON M1R 5G1 Tel: (416) 899-1882 Fax: (905) 882-8812 www.sentec.ca -----Original Message----- From: Chris Mahanna <[log in to unmask]> Date: Fri, 12 Feb 2010 16:16:07 To: <[log in to unmask]> Subject: Re: [TN] Die cracks Thanks again to everyone. To be safe, it looks like we'll be running a little experiment with Sonoscan. I've got permission to post what we find. Chris -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Chris Mahanna Sent: Friday, February 12, 2010 2:59 PM To: [log in to unmask] Subject: Re: [TN] Die cracks Hi Vlad, Thanks Trust me, this is what we want the answer to be. And yes we do approach with 180 or 320. But why do we see it in only 0.1% of our BGA sections? And is it our process that grouped the observations with these samples? And, just to be clear, do you know the signature? We know the edge grinding damage signature: https://robisan.sharefile.com/d-s441418b99d34882b Chris -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev Sent: Friday, February 12, 2010 2:18 PM To: [log in to unmask] Subject: Re: [TN] Die cracks Chiris, 99.999999% the cracks are due to the sample preparation. Most probably, the die was approached (touched) with a low drig SiC paper (like 180), -- Best regards, Vladimir mailto:[log in to unmask] SENTEC 11 Canadian Road, Unit 7. Scarborough, ON M1R 5G1 Tel: (416) 899-1882 Fax: (905) 882-8812 www.sentec.ca ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________ --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ______________________________________________________________________ This email has been scanned by the MessageLabs Email Security System. For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________