Bill, You wrote: Solder is only 7.5 times worse than the copper?... compared to CB1 at 77 times ... and Air which is 388 times... The solder is almost 800 Percent worse as a conductor of heat. Air thermal conductivity depends on temperature but is about .027 W/m k or about 14,000 times worse than copper. Sounds like a lot but those are the numbers I found with a quick look on the web. Yes copper is about 8 times more conductive of heat than solder. A lot depends on the hole size. A .014 hole plated at 1/2 oz exposes a copper cross section about 1/5 the hole surface area. As the hole gets larger they rations grow by a square. At about 40 mil hole the rotten solder conducts almost twice the heat as the copper wall. If anyone can correct these numbers please let me know. Filling a few vias with selective solder or wave is not that difficult. Protos are easy build by hand. Filling the vias with air is easy and cheap. Solder filling is better, it almost buys you twice the thermal conductivity for a small hole (.014) and a lot more conductivity at larger holes. Has anyone seen any small copper studs that can be placed and soldered using pin and pasts techniques? That would really conduct some heat! Bob Kondner -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Brooks, Bill Sent: Monday, January 04, 2010 5:08 PM To: [log in to unmask] Subject: Re: [TN] Thermally Conductive & Plated Via Fill Thanks for the comments... As far as my personal limited experience goes for plating vias shut... we don't reject for it... but we have not seen any vendors actually plate them shut so maybe they don't like to do that either... Like you say Chris... it's probably not a good practice with conventional methods. We typically use a 14 mil plated thru hole with a 24 mil pad... but for thermal vias I have used .008 in. holes (2mm) with a 18 mil pad. Of course larger boards would have reduced Producibility due to the tolerances but all things are compromises... I have attended a couple of lectures on plated copper filled vias and there are a few companies that claim to be able to make fully copper filled vias with a proprietary plating process that yields something like a solid 'copper pillar' thru the board. The sections under microscope looked very impressive... I don't have the thermal analysis numbers we did here handy but should we really describe the solder performance as 'Not that bad'? Solder is only 7.5 times worse than the copper?... compared to CB1 at 77 times ... and Air which is 388 times... The solder is almost 800 Percent worse as a conductor of heat. If the majority of the medium thru which you transfer heat is solder... you have a big resistance between the heat and the ambient air... which btw will make the junction temp rise significantly over a thicker copper solution. The solder would be the biggest resistance in the path... if the copper is only 1 mil thick at the walls of the via... the solder is the remainder of that volume... so which material by volume has the biggest influence on temperature rise? Add to that thought... bubbles or voids in the solder... hmmm. Thermal dynamics as you know is not a simple comparison problem... I could have the best possible conduction thru the board and put a 'not that bad' thermal pad on the back side of it between it and the metal plate and still have the part fail from overheating at the specified ambient temps required. Each thermal junction from the heat source to the ambient air is a thermal resistance... and they all add up. The highest resistance in the path is the limiting factor...making the whole system worse. You must look at all the thermal resistances between the heat source and ambient air to calculate the projected junction temps at the source semiconductor and the temps that the board is going to be exposed to. Not to mention the effect of surrounding heat sources that are also in the area of the part contributing to the heat load that needs to get to ambient to protect the board and the components from over heating... Each component needs to be looked at together as a system... The amount of copper in the hole is just one part of the heat path equation and system for getting the heat out. Solder... according to your numbers, is much worse a thermal conductor and is not helping the heat transfer load much... and would be much better replaced by copper if possible... of course. CB-100 sounds more like and insulator than a conductor of heat. Maybe good as spackling compound... (Drywall putty) it gets the hole closed... so it's 'better' than air. But all of the 'significant' heat transfer is being conducted thru the copper plated walls of the thermal vias... in either case :) Best regards, Bill Brooks | Datron World Communications, Inc. PCB Designer/Engineer | Office: 760-602-7004| Fax: 760-597-3777 | [log in to unmask] 1808 Aston Avenue, Suite 230, Carlsbad, CA 92008 | www.dtwc.com Performance You Require. Value You ExpectTM -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner Sent: Monday, January 04, 2010 12:12 PM To: [log in to unmask] Subject: Re: [TN] Thermally Conductive & Plated Via Fill Bill, Compared to copper solder is a poor thermal conductors but it is not all that bad. A quick check shows: (W/m-C) Soft Solder = 51 Copper = 388 CB-100 = 5 But a simple via hole can have a pretty big area. Solder is a lot less expensive and conducts heat 10 time better then CB-100. Filling vias with solder could be a big help in many applications. Thanks, Bob Kondner --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------