Hi Victor, This is one of the problems with HALT—it is so severe and unconnected to real use conditions, that you can get failure indications that are not pertinent to the reliability of your product. You really should have used IPC-9701. Now you do not know whether or not you have a problem. In terms of partial cracks and failure definition, you may want to ookl at my column in the January issue of Global SMT & Packaging. Werner -----Original Message----- From: Victor Hernandez <[log in to unmask]> To: [log in to unmask] Sent: Fri, Dec 18, 2009 10:45 am Subject: [TN] Solder Joint Fracture Fellow TechNetters: What is IPC position on a solder joint fracture on a gull wing connection. What percentage of fracture on the IMC region and/or bulk solder is permissible? Post Reliability, HALT. Victor, --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------