If you found it at inspection prior to your reliability testing, it is a defect. Because you found it post-test, it is still a defect per IPC 610D, but it is also a reliability issue and must be dealt with. You need to determine root cause and correct the process or design issue leading to the cracks. R. Dean Stadem Consulting Engineer Analog Technologies Corp./Lumagine, Inc. 11441 Rupp Drive Burnsville, MN 55431 (952)894-9228 [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez Sent: Friday, December 18, 2009 9:45 AM To: [log in to unmask] Subject: [TN] Solder Joint Fracture Fellow TechNetters: What is IPC position on a solder joint fracture on a gull wing connection. What percentage of fracture on the IMC region and/or bulk solder is permissible? Post Reliability, HALT. Victor, --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------