Guy, It's Friday and I have cold DEW in my hand so I'll use Doug's typical answer, it depends. Our experience is that intermetallics are strong but brittle and cutting and prying packages is likely to cause an impact on solder joints that do fracture at intermetallic interfaces. Do you know what the surface finish is on the packages your customer is using? Regards, George George M. Wenger Andrew Wireless Solutions Senior Principal FMA / Reliability Engineer 40 Technology Drive, Warren, NJ 07059 (908) 546-4531 [Office] (732) 309-8964 [Mobile] [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey Sent: Friday, November 20, 2009 3:28 PM To: [log in to unmask] Subject: [TN] solder fracture solderable? I was visiting a customer earlier this week. They were attempting to cut a the top part off of a package on package, BGA on top of BGA. They didn't want to reflow it off because they didn't want to damage the balls on the bottom of the bottom package. They had made a little fixture affair with two knives adjusted to slice between the two packages. They placed the PoP in the tool and pushed it through the knives, rotated 90 degrees and repeated the cycle. Most of the pads on top of the bottom package ended up with half a ball remaining on the pad. But some of the pads did not have any solder on them at all. The entire pad was mat finish silver in color. None of these features would accept solder. The number of pads without solder varied from one or two to 30% of the pads. I wondered if rather than cutting through, some of the connections has simply fractured along the intermetallic, leaving a non-solderable surface with this uniform appearance. Some of those observing conjectured that the package was bad, They conjectured that the silver was merely solder loaded with gold and that the nickel had never accepted solder. I asked where their SEM was and if they had EDAX equipment . . . nope. Would anyone care to guess along? How likely is it that prying off a BGA would fracture the connection right along the intermetallic and leave a completely non-solderable surface? --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------