Hi, The other week there was talk about ENIG vs HASL so I have been searching around the web for ENIG info. I read a number of items. I recall reading that a phosphorus (in nickel) content of > 10% (I think it was %) was required to control the Immersion Gold thickness and better control corrosion resistance. Wow, 10% sounds high but I guess that is right. The photos show a P+ layer at the failed interface. Does that imply increasing P is a problem at making "Strong" soldered connections? How does a lowly PCB user monitor this kind of parameter of phosphorus so it is not too much or not too little? Or did I misread the entire scenario? Thanks, Bob Kondner -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Monday, November 23, 2009 2:31 PM To: [log in to unmask] Subject: Re: [TN] solder fracture solderable? Hi Inge, Sorry it took me a while to get this posted, I've been doing assembly quotes a good part of the morning. Yeah, Guy has quite the story to tell about his adventure, wish I could talk about it, but then he would have to kill me... But anyways here's your pics: http://stevezeva.homestead.com/Image1.jpg http://stevezeva.homestead.com/Image2.jpg http://stevezeva.homestead.com/Image3.jpg http://stevezeva.homestead.com/Image4.jpg http://stevezeva.homestead.com/Image5.jpg Steve -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar Sent: Monday, November 23, 2009 6:52 AM To: [log in to unmask] Subject: Re: [TN] solder fracture solderable? I don't believe in the knife idea. Have my own way. Complicated, but works (not always). 1. Cut out the area of interest (e.g. BGA) with good marginal. Use fine blade diamond saw. Let it take time. Use cutting oil. 2. Clean from oil. Glue mount two thick metal plates to both sides of the sample under test. Each plate has a hook attached to the plate. 3. Place the sample in at pull tester and pull apart until the BGA separates from the board. Use low speed. I've sent example on this to Steve Gregory. /Inge -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Guy Ramsey Sent: fredag 20 november 2009 21:28 To: [log in to unmask] Subject: [TN] solder fracture solderable? I was visiting a customer earlier this week. They were attempting to cut a the top part off of a package on package, BGA on top of BGA. They didn't want to reflow it off because they didn't want to damage the balls on the bottom of the bottom package. They had made a little fixture affair with two knives adjusted to slice between the two packages. They placed the PoP in the tool and pushed it through the knives, rotated 90 degrees and repeated the cycle. Most of the pads on top of the bottom package ended up with half a ball remaining on the pad. But some of the pads did not have any solder on them at all. The entire pad was mat finish silver in color. None of these features would accept solder. The number of pads without solder varied from one or two to 30% of the pads. I wondered if rather than cutting through, some of the connections has simply fractured along the intermetallic, leaving a non-solderable surface with this uniform appearance. Some of those observing conjectured that the package was bad, They conjectured that the silver was merely solder loaded with gold and that the nickel had never accepted solder. I asked where their SEM was and if they had EDAX equipment . . . nope. Would anyone care to guess along? How likely is it that prying off a BGA would fracture the connection right along the intermetallic and leave a completely non-solderable surface? --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------