Hi Peter, You give us precious little to go on. Open Q's—(1) is it a soldering or solderability problem—have you actually formed a SJ, you need more thermal energy soldering to Ni because of the slow dissolution rate; (2) is the NI-plating thick enough or does it get consumed in the soldering; (3) does the Ni-plating have a good metallurgical bond to the actual clip metal. That external lab should have been able to answer your Q's, but commercial labs typically do not interpret what the found except in relationship to standards—and this is clearly non-standard. Werner -----Original Message----- From: Peter L <[log in to unmask]> To: [log in to unmask] Sent: Fri, Oct 30, 2009 12:54 am Subject: [TN] Solderability issue with nickel plated battery contacts Hi technet, We have run into solderability issues with a major battery clip supplier. The battery clips are SMT on the board which then get installed into a remote control hand held shell. After SMT reflow the clip will shear off after slight push with a finger. External lab analysis (cross sectioning, solderability test) indicated internal nickel separations hence the nickel plating process was not robust and tightly controlled. After months of investigation we see impoved results but still failures. Has anyone else experienced this type of issue before? We are evaluating different options including a change of vendor. Can someone share what they have been using in these type of application? Appreciate any comment. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------