Hi Bill, George's questions are important. ENIG 'Black Pad' happens mostly to people [that is, suppliers & users] new to ENIG. You do not give enough details, so a proper diagnosis is impossible at this stage. Werner -----Original Message----- From: [log in to unmask] To: [log in to unmask] Sent: Tue, Oct 20, 2009 7:21 pm Subject: [TN] ENIG Issue Fellow TechNetters: I ran into a problem and I am looking for more information. We had some PCB made with ENIG for SMT applications. We populated the backside, ran them through the convection oven, the solder fillets were fine. Populated the first five (5) PCBs on the topside, ran them through the convection oven, and the solder fillets were quite bad, actually dewetted. Could not even be touched up. Tried two (2) more random PCBs and got the same results. Never have run into this before but have been told it is NOT a unique problem. Has anybody had this happen? Have to tell our customer that they are not going to be getting their PCBs on time and would rather not look like the north end of a southbound mule. Thanks in advance for your assistance. Bill Black 1 631 667 9699 X13 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------