It is a common practice to double coat solder mask for heavy oz outer layer copper. However, functionally or cosmetically, double coat shall be better than or as good as single coat. So there is no excuse for bubbles or stringers. Their double coat process is not optimized yet. Regards, Jason Zhao -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of J W Sent: Thursday, October 29, 2009 7:41 AM To: [log in to unmask] Subject: [TN] Bare Board Quality (mask issues) Hi, Looking for some expertise regarding bare board fabrication and the solder mask process. We have a supplier (China) that decided to add two layers of mask versus one layer (not called out in our specifications). The reason for doing this is explained by them below. Our end customer does not like the two-layer mask and thought it was due to a rework process. I am not familiar with a two-layer solder mask process, is this something new? Is this OK? Their solution is to not do it anymore, but I want to understand is this something others have seen and approved. If so, why? In addition, during this two layer process, they say they will have air bubbles (note 2 below), which we found in a cross section. They wrote that going to one-layer would eliminate the air bubbles? Not sure if that is true or if their process is questionable. Lastly, we also found thin solder mask stringers stretched across some pads. They claim dirty worktable (note 3 below) I wonder if this was caused by the extra solder mask layer application? I appreciate any comments. Thanks, Jim * COMMENTS FROM SUPPLIER A1: (1) Supplier adopted twice solder mask coating process to produce this PCB. They are NOT reworked PCB. As the copper thickness of this PCB is 2OZ , Supplier adopted twice solder mask coating process based on below conception. a: Considering the working power will be huge when PCBA's working, to perform twice solder mask coating process will enhance PCB quality and prolong PCB cycle life, preventing solder mask being broken down if the solder mask aging after long time usage b: As usage frequency of this PCB is higher than general PCB, adopting twice solder mask coating process will prevent outside signal interferer for PCB when the solder mask's aging. (2) As adopt twice solder mask coating process, solder mask is too thick(within 60~70um), the air bubbles in the solder mask is difficult to get away (3) The stringers on pad is caused by adhering foreign stuff from worktable before OSP process."* --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------