George, ABSOLUTLY right!!!!!! Vladimir SENTEC 11 Canadian Road, Unit 7. Scarborough, ON M1R 5G1 Tel: (416) 899-1882 Fax: (905) 882-8812 www.sentec.ca -----Original Message----- From: "Wenger, George M." <[log in to unmask]> Date: Tue, 20 Oct 2009 21:03:58 To: <[log in to unmask]> Subject: Re: [TN] ENIG Issue George, Not everyone links solderability issues with ENIG to "Black Pad". In my email to Bill I didn't use those two words primarily because I believe they describe an appearance and not a failure mechanism. Regards, George George M. Wenger Andrew Wireless Solutions Senior Principal FMA / Reliability Engineer 40 Technology Drive, Warren, NJ 07059 (908) 546-4531 [Office] (732) 309-8964 [Mobile] [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of George Milad Sent: Tuesday, October 20, 2009 9:52 PM To: [log in to unmask] Subject: Re: [TN] ENIG Issue As always as soon as there is a solderability issue with ENIG, "Black pad" comes up. This is a problem because it does not allow for further investigation. Everyone accepts since this is ENIG then it must be black pad. If this was a black pad issue the back side should have exhibited the same problem. BP occurs during the plating of the gold on top of the Ni. BP cannot differentiate one side from the other. Do not accept BP as the answer and keep investigating. Regards George Milad George Milad National Accounts Manager for Technology Uyemura International Corp (UIC) 249 Town Line Rd Southington CT 06489 [log in to unmask] Cell: (516) 901 3874 --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------