Good morning, We have an application where we use 1/2 inch thick G-10 as an insulator and we are finding that the machined edges are porous which is allowing a thermal transfer wax to soak into the material and cause us to fail hi-pot. We have discussed coating all sides of this thick material with LPI or conformal coating. The temperature range of operation is typically a maximum of 70° C and the location is in a piece of equipment in a doctor's office. We are looking for a cost effective and simple solution for this low volume product (currently under 200 pieces per year). Thanks in advance, Phil Nutting Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender. If you have received this email in error, please immediately return it to sender and delete the copy you received. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------