Lamar, a good example on how to get help.I just filled in' ASTM D3359' and it took just 5 seconds to get this answer: http://listserv.ipc.org/scripts/wa.exe?S2=TECHNET&D=0&H=0&O=T&T=0&q=ASTM+D3359&s=&f=&a=&b= Inge ----- Original Message ----- From: "Lamar Young" <[log in to unmask]> To: <[log in to unmask]> Sent: Wednesday, September 02, 2009 5:49 PM Subject: [TN] Adhesion tape test >I need help finding a suitable replacement tape to perform adhesion > testing per ASTM D3359, the tape test method. > > The Permacel 99 tape that was mentioned is no longer available. We have > tried a replacement tape recommended by a tape vendor, but the backing > released from the adhesive during the test (the adhesive stuck better to > the substrate than the backing). > > Any help would be much appreciated. > > Lamar > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------