Hi Charles,
If you can not prevent the
solder ball appear in you process well, you can clear out the solder ball with ESD
brush in you touch up station after wave solder process to meet IPC standard.
Maker.
From: TGAsia
[mailto:[log in to unmask]] On Behalf Of Charles
Lee(SVA)
Sent: Wednesday, August 19, 2009
11:03 AM
To: [log in to unmask]
Subject: [TGAsia] Solder Balls
Dear All,
There are a great deal of tiny solder balls appeared
in around PTH connector pins after wave soldering (PB Process) , please see the
attached pictures.
Here we would like to seek your helps and suggestions on
how to solve the solder ball issues, thanks!
Best regards
Charles Lee