Inge, I am not sure which method/process is being used on the notebook battery spot weld. IMHO, there must be some type of guideline for acceptability. Optically, one of the metal leaves/foil material reflowed at the interface an left an open arch. Somewhat difficult to explain. I will attempt to post a photo for all to see. Victor, -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Sent: Tuesday, August 25, 2009 2:49 PM To: [log in to unmask] Subject: Re: [TN] Metal spot weld, cylindrical battery end terminal Victor, spot what? Capacitor discharge or resistance weld or laser or friction or ... Inge ----- Original Message ----- From: "Victor Hernandez" <[log in to unmask]> To: <[log in to unmask]> Sent: Tuesday, August 25, 2009 9:41 PM Subject: [TN] Metal spot weld, cylindrical battery end terminal Fellow TechNetters: Can someone share their experience with spot weld guideline as view optical and with x-ray. Victor, --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------