Hi Wayne, Probably 60% of what we build these days is electroplated gold, but buss bars are not allowed nor is pattern plating - we have to plate up through the vias and then do a secondary etch- somewhat painful but not excessively so. Regards Steve Kelly -----Original Message----- From: Thayer, Wayne - IIW [mailto:[log in to unmask]] Sent: August-04-09 1:17 PM To: TechNet E-Mail Forum; Steve Kelly Subject: RE: [TN] Wire bond Gold bonding requires electroplated gold. Either the electroplating will be done with "buss bars" or the outer layers will be pattern plated with gold. If pattern plating, the gold stays there, and you will have under-cutting of the pads which will be at least as much as the thickness of the copper under the gold. Not many fabs know how to check that, so most stuff comes out way over-etched (but that nice gold on the surface looks great--until it falls off!). Aluminum bonds to copper just fine, so this isn't an issue. Even ImAg works pretty well to protect the copper from oxidation. But wedge bonding has its own issues--decreased speed, more brittle wires, more difficult looping, etc.) Wayne Thayer -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Kelly Sent: Tuesday, August 04, 2009 1:02 PM To: [log in to unmask] Subject: Re: [TN] Wire bond Hi Joyce, Do not understand your response - why would a .002 etched pad be flatter in the centre - I have done thousands of x-sections and SEMS - never seen this. Why would I have exposed copper at an edge- never built a wire bond circuit that would have that issue. Regards Steve Steve Kelly PFC Flexible Circuits Limited PH: (416) 750-8433 Fax: (416) 750-0016 Cell: (416) 577-8433 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo Sent: Tuesday, August 04, 2009 12:56 PM To: [log in to unmask] Subject: Re: [TN] Wire bond Yap. The flatness of the center pads is better than the edge, just in case you have some exposed copper at the edge, that will harden the gold locally. -------------------------- Sent using BlackBerry ----- Original Message ----- From: TechNet <[log in to unmask]> To: [log in to unmask] <[log in to unmask]> Sent: Tue Aug 04 11:36:30 2009 Subject: [TN] Wire bond Good Morning, Does the size of a wire bond pad (in this case with a perfect etch .002 wide) have any effect on whether the wire bonder does Al wedge or Thermosonic gold( I know the gold plating is different) - just asking about the process. Thanks. Steve Kelly Steve Kelly (PLEASE NOTE NEW E-MAIL ADDRESS) (416) 750-8433 (work) (416) 750-0016 (fax) (416) 577-8433 (cell) --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------