I would not use cross hatching in modern high-speed or RF designs, cross hatching is ok for designs that have no high-speed though. We are to the point of taking the tightness of the prepreg weave into consideration for impedance issues so a cross hatched reference plane is defiantly out of the question today. To your question, the only issue I have ever seen, and continue to see, is warpage of unbalanced layers. Use outer layer thieving pads and balance inner layers to avoid this and you will be ok. Even the outer layer thieving is optional but I do it as often as I can. (some customers hate seeing it) It's not very scientific, if you have a 6 layer PCB and layer 2 is a solid plane then make sure that layer 5 (at least) closely resembles. Ken _____________________________________ Kenneth J. Wood Saturn PCB Design, Inc. [log in to unmask] www.saturnpcb.com -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis Sent: Thursday, July 30, 2009 4:03 AM To: [log in to unmask] Subject: Re: [TN] Hashing-Out Hatching In my former lives, last century, I always cross-hatched, especially on inner layers. Never any problem with imbalance, better adhesion of solder mask, less risk of delamination etc. I still applied thermal breaks etc. The CAD package I used gave free choice of width/space dimensions. Testing of characteristic impedance over cross hatching revealed absolutely no difference or reflections (thickness of dielectric in our case ~0.3 mm), provided the space between the hatches was less than the dielectric thickness. Another point I found is that a client had massive solid planes with 105 µm copper on inner layers for a power application (hairy at best!!!). During pressing, he tended to have resin starvation, as it flowed to fill where there was no plane. He changed to a low-flow resin and didn't have enough in the non-plane areas. I advised cross-hatching with 5 mm width/space: no further problem and he still had enough copper to pass the curremt. IMHO, it has everything going for it and nothing against it. Brian James Head wrote: > I'll use hatched planes occasionally, to "even" etching across the board > material, but only on mixed plane/signal layers. It depends upon the > board, how much copper tracking and plane area is on the board and in > what areas. > > James > > ******************************************************** > > The information transmitted is intended only for the person or entity to > which it is addressed and may contain confidential and/or privileged > material. If you are not the addressee, any disclosure, reproduction, > copying, distribution, or other dissemination or use of this transmission in > error please notify the sender immediately and then delete this e-mail. > E-mail transmission cannot be guaranteed to be secure or error free as > information could be intercepted, corrupted lost, destroyed, arrive late or > incomplete, or contain viruses. > The sender therefore does not accept liability for any errors or omissions > in the contents of this message which arise as a result of e-mail > transmission. If verification is required please request a hard copy > version. > > ******************************************************** > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------