Then it's probably not red P, because this was earlier. And I never heard Interseal's name mentioned. But...we don't know from whom Interseal buy their mold material, so what you can do is frankly call them and ask if they have had red P problem. If they have, they will probably try to avoid a straight answer. In the end, you have to do own research. Note, what I say is a proposal, there are other explanations, locked-in humidity being one such. Inge ----- Original Message ----- From: "Toby Carrier" <[log in to unmask]> To: <[log in to unmask]> Sent: Friday, July 17, 2009 8:20 PM Subject: Re: [TN] ESD failure difference between 16-QSOP and 16-SOIC Video Buffer Inge, The manufacturer is Intersil, EL5308. The datasheet states May 3, 2007. Toby --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------