Hi Dennis, That's pretty slick, do you have any captures that you could send to Steve to post? KennyB -----Original Message----- From: Dennis Fritz [mailto:[log in to unmask]] Sent: Friday, July 24, 2009 1:11 PM To: [log in to unmask] Subject: Re: [TN] PCB Inspection - with added E-bay "digital microscope" Now this is the Purdue Technology Center Summer Intern "patent-pending" ?inspection device for tin whiskers. Steve, please post to your web site for IPC pictures.? Here is the link to Ebay for more of these $50 digital microscopes. Remember, there is no vernier on here to measure distance. Also, the price went to $49.99!!! --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------