John: Ignoring what is written in any specifications, and what is in the customers mind, the bottom line is this: You will get cleaner parts in an aqueous, NON-ULTRA SOUND, cleaner than you will in alcohol in ultra-sound. And, it will be much less costly, even if you avoid a "flaming incident", and one helluva lot faster. Is your customer able to approve, or reject parts which have been cleaned? Can you clean some parts "your way", and submit for approval? What are parts made of, and do you have tests to prove/disprove cleanliness? We have developed some tests for certain metals which prove/disprove cleanliness. The tests are qualitative, but VERY sensitive. Rudy Sedlak RD Chemical Company --- On Mon, 6/29/09, John Anselmo <[log in to unmask]> wrote: From: John Anselmo <[log in to unmask]> Subject: Re: [TN] IPA o r Methanol in Ultrasonic Cleaner To: [log in to unmask] Date: Monday, June 29, 2009, 10:16 AM Hi Bev, To answer your questions: Approximately half a dozen of each (screws/washers/ etc. The qty is for each assembly and they only need to be cleaned before final assembly, so it will be an ongoing process. We are trying to clean any contaminants (oils) on the machined parts. I haven't researched what finish will be on the screws yet. John -----Original Message----- From: Bev Christian [mailto:[log in to unmask]] Sent: Monday, June 29, 2009 9:34 AM To: TechNet E-Mail Forum; John Anselmo Subject: RE: [TN] IPA o r Methanol in Ultrasonic Cleaner John, Well part of this (safety considerations) will vary from jurisdiction to jurisdiction. Second, How many screws and how often? Is this once off or will it be repeating? Third What is it you are tying to clean off? Fourth Are the screws painted, chromated, etc.? Bev RIM -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of John Anselmo Sent: Monday, June 29, 2009 11:27 AM To: [log in to unmask] Subject: [TN] IPA o r Methanol in Ultrasonic Cleaner Technet, We are being asked by one of our customers to clean some parts (screws, washers, standoffs, feedthrus) in an ultrasonic cleaner with either Methanol or IPA (spectroscopic grade). The time in the ultrasonics could be up to 1 hour. Does anyone else have experience and recommendations for doing this? My main concern is safety. What type of room or enclosure do we need for this? Thanks, John Anselmo --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------