Mike, it is ok to rant in this forum, you are bringing up some good points in doing so. My customer representative in this case is a very sharp man who is responsible for a program that demands the most rigorous quality controls possible. I actually don't fault him for demanding some type of point-of-use quality check on the solder paste even in the face of a complete supply-line quality plan that should otherwise be air-tight, so to speak. I am just looking for other opinions as to what the point-of-use check could or should reasonably include. -----Original Message----- From: Mike Fenner [mailto:[log in to unmask]] Sent: Wednesday, June 24, 2009 11:01 AM To: 'TechNet E-Mail Forum'; Stadem, Richard D. Subject: RE: [TN] Solder paste validation at point of use Your customer is a little behind the times, [but then he is the customer.] People used to do this to try to find good product in the stuff they received and/or find the number that corresponded to the good stuff. As you know few paste problems are to do with as received viscosity, and a half decent operator using a MK1 Eyeball and $2.00 spatula will spot them anyway. These days most people's objective is to have products that are ship to line, including paste, and that is possible. In Europe we have a small handful of people who check our viscosity, and that's a generous assessment. I imagine the same in RoW. Viscosity checks usually cause grief because few users are prepared to pay for a decent viscometer or trained staff, so the as-received measurement is apparently different to the as-shipped. Question: why would we, or anyone else for that matter, measure something find it wrong, and then ship it anyway. Especially to someone we know is going to check it? Sorry I am ranting a bit... If you need to do a test I suggest a simple print and reflow test, using a spare area [on the unseparated panel] of your production boards. This can be printed up with a line of varied pitch dots. You can check print quality, coalescence and spread, the test also verifies solderability of board. Bob Willis has a chart or something on this which explains it all. Regards Mike Fenner Indium Corporation T: + 44 1908 580 400 M: + 44 7810 526 317 F: + 44 1908 580 411 E: [log in to unmask] W: www.indium.com Pb-free: www.Pb-Free.com --------------------- Indium Corporation Incorporated in New York, USA Registered office: (Not for correspondence) 77-97 Harpur Street, Bedford , UK Registered number: fc16473 -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D. Sent: Wednesday, June 24, 2009 3:22 PM To: [log in to unmask] Subject: [TN] Solder paste validation at point of use I would like to know what others do to ensure that the solder paste is good at the point of use. I am NOT looking for a solder paste handling procedure, what I am looking for is what type of test can be performed that is quick, easy, and does not hold up production. We do paste viscosity testing on each lot that we receive, and we also strictly monitor our paste printing process with the post-print inspection machine. We have validated our entire solder paste handling system to ensure that the paste is handled, labeled, and properly rotated. We have had no issues with the solder paste that we use. Our customer thinks we should test each lot of paste when it is removed from refrigeration prior to use on production hardware. I am not really sure what a second viscosity check would do for us, but I am open to some other testing method that does not consume a lot of paste and would provide data we can use. Any suggestions? --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited. Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.*** --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------