Solder mask defined pads or non-so Electrolytic Ni-Au or ENIG? Solder mask defined pads or non-solder mask defined pads? Has any ionic contamination measurement been done of the PCB before assembly? All of the above questions are asked to determine if there is any plating chemistry trapped that isn't cleaned off before assembly. However, when the customer indicates they don't see the Sn migration with SnPb assembly I'd go back to your statement earlier about the flux-vehicle in the SAC solder paste is most likely different than for the SnPb paste and has to be considered a suspect. Regards, George George M. Wenger Andrew Solutions Senior Principal FMA / Reliability Engineer 40 Technology Drive, Warren, NJ 07059 (908) 546-4531 [Office] (732) 309-8964 [Cell] [log in to unmask] -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Karen Tellefsen Sent: Friday, June 12, 2009 1:19 PM To: [log in to unmask] Subject: Re: [TN] Strange tin "migration" under OFN soldered with no-clean SAC305 solder paste More information from our tech service engineer: There is no hand soldering. The board is Ni-Au The boards are clean... no issue with Sn Pb Could it be galvanic corrosion with exposed Ni or Au acting as a cathode, allowing the tin in the solder joint to corrode? Maybe there is some metal surface on the QFN that can act as a cathode. There's no externally applied voltage, maybe there is a battery somewhere on the board. Karen Tellefsen - Electrical Testing [log in to unmask] 908-791-3069 Dave Hillman wrote: Hi Karen - you should attempt to determine if any ionic contamination is present - you could just have a typical electrochemical migration issue to due contamination. Dave Hillman Rockwell Collins [log in to unmask] Karen Tellefsen <[log in to unmask]> Sent by: TechNet <[log in to unmask]> 06/12/2009 11:12 AM Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to Karen Tellefsen <[log in to unmask]> To [log in to unmask] cc Subject Re: [TN] Strange tin "migration" under OFN soldered with no-clean SAC305 solder paste I'm not sure; I'm getting my information second hand. Thanks ------------------- Karen, Are you sure this is migration? They might very well be plain shorts from excess of solder or manual component realignment before reflow. Has the assembler checked the components under X-Ray before the conditioning, just to make sure everything is clean at the exit of the oven? Just a thought, Ioan Tempea, ing. t : 450-967-7100 ext : 244 [log in to unmask] www.digico.cc P N'imprimer que si nécessaire - Print only if you must ----- Forwarded by Karen Tellefsen/AlphaMetalsUS/Cookson on 06/12/2009 10:47 AM ----- Karen Tellefsen/AlphaMe talsUS/Cookson To [log in to unmask] 06/12/2009 10:26 cc AM Subject Strange tin "migration" under OFN soldered with no-clean SAC305 solder paste One of our technical service engineers asked me about a strange migration phenomenon one of our customers observed under passives and QFN's that have been soldered with one of our no-clean SAC305 solder pastes. I've attached an X-ray picture of a QFN exhibiting this strange failure, but I don't know how it can be posted so you can look at it.. Further analysis after removing the component showed that the shadows in the X-ray picture is caused by a black material containing tin. The boards were conditioned 85°C 85%RH for 500 hr, but no voltage was applied. This phenomenon was not observed under QFPs (not surprising), and seems to be independent of reflow profile used. Additionally, the customer has not seen anything like this with tin lead solder paste, however, the tin-lead solder pastes would have a different fluxes. The tin "migration" is coming from both adjacent solder joints, and there is no voltage applied, so it seems to be a corrosion problem. Certainly QFN and big passives are good at trapping and retaining water in the flux residue underneath them. I've never seen anything like this; has anyone else out in TechNet land seen this or have any ideas what caused this? Thanks Karen Tellefsen - Electrical Testing [log in to unmask] Enthone GmbH Geschäftsführer: Knut Balzer, Luc de Croo, Jürgen Dietrich Amtsgericht Düsseldorf HRB 45276 USt-Id-Nr. DE 811 205 946 This communication is for use by the intended recipient and contains information that may be privileged, confidential or copyrighted under applicable law. If you are not the intended recipient, you are hereby formally notified that any use, copying or distribution of this e-mail, in whole or in part, is strictly prohibited. Please notify the sender by return e-mail and delete this e-mail from your system. Unless explicitly and conspicuously designated as "E-Contract Intended", this e-mail does not constitute a contract offer, a contract amendment, or an acceptance of a contract offer. This e-mail does not constitute a consent to the use of sender's contact information for direct marketing purposes or for transfers of data to third parties. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- ------------------------------------------------------------------------------------------------ This message is for the designated recipient only and may contain privileged, proprietary, or otherwise private information. If you have received it in error, please notify the sender immediately and delete the original. Any unauthorized use of this email is prohibited. ------------------------------------------------------------------------------------------------ [mf2] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------