I remember searching the TN archives on this issue some time ago, and the consensus seemed to be that flux-cored Sn63Pb37 solder should last pretty much indefinitely. The flux core is sealed in very well, though the flux may be compromised a short distance in from the severed end of the wire. Oxide formation on the outside of the solder shouldn't be an issue either. This may not hold for high tin or lead-free solder alloys. -Joe -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory Sent: Friday, June 05, 2009 11:38 AM To: [log in to unmask] Subject: [TN] Flux cored wire solder shelf life Well, we made it to Friday! I'm going ask ya'll a couple of question that I think I know the answer to, but I want to hear what you think. Right now I'm in the midst of gathering up all my solder dross, expired solder paste, and wire solder for a shipment to my recyclers. I noticed we had a bunch of wire solder in the locker of our training room that was really old, like it was manufactured back in February of 1997. The alloy is 63/37, the flux core is a pretty active water soluble organic acid. The manufacturer says that shelf life for flux cored wire solder is 3-years. But when I took some of the solder and soldered with it, it soldered absolutely fine. Wet and flowed out with no problems whatsoever. So my question is, have any of actually had any problems soldering with flux cored wire solder because it was too old? Do you think that manufacturers shelf life is realistic? Steve --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------