The thing that shocks me is not the desire to distill IPA but the fact that you USE IPA before conformal coating. It is not a good defluxer. Distillation is not easy. The Black Foresters gather cherries and put them in large tubs for a few weeks and then distill the fermented juice. They never get pure alcohol, but a deliciously perfumed eau-de-vie called Kirschwasser with a distinct aroma of the cherries it was derived from. Why? Because of azeotropes. Even a mixture of ethanol and water will not distill into pure alcohol but into a mixture of about 96% EtOH. Rudy mentions esters; these are the reaction products between alcohols and acids and it is what gives Kirschwasser its aroma and flavour. Esters usually form azeotropes with alcohols and it is not impossible for raw organic acids to do so as well. So distillation may remove most of the rosin but the resultant juice may not be brilliant as a safe defluxer, possibly even worse than not cleaning at all. Apart from which, alcohol vapours and air can form a highly explosive mixture. H&S regulations would require you to install such a still in an explosion-proof bunker KABOOOOM! Brian Kane, Amol (349) wrote: > I am looking for some information from people who own a alcohol distillation unit that converts alcohol waste (alcohol + fluxes etc.,) into usable alcohol again. I know that such a unit exists, but need to talk to people who actually use it. We are trying to limit the amount of IPA waste we generate from clean boards prior to CC. > > Offline replies are welcome too. > > Thanks and regards, > Amol > > > > WARNING: Export Control > This document may contain technical data within the definition of the > International Traffic in Arms Regulations (ITAR), and subject to the Export > Control Laws of the U.S. Government. Transfer of such data by any means to a > foreign person, whether in the United States or abroad, without proper export > authorization or other approval from the U.S. Department of State is > prohibited. > > CONFIDENTIALITY NOTICE: > This e-mail, and any attachments, is for the sole use of the intended > recipient(s) and may contain information that is confidential and > protected from disclosure under the law. Any unauthorized review, use, > disclosure, or distribution is prohibited. If you are not the intended > recipient, please contact the sender by reply e-mail, and delete/destroy > all copies of the original message and attachments. > Thank you. > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 > ----------------------------------------------------- > --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------