Yes, if you have a paste flux and reflow profile that leave the land and BGA ball interface after reflow is achieved. If the flux leaves any of the ball-pad interface too early in the process you can get opens. Because there is marginally less solder the joint is a little weaker. But, in my experience, it isn't enough to matter. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Kelly Sent: Wednesday, June 03, 2009 12:10 PM To: [log in to unmask] Subject: [TN] BGA-113 package Hi All, We have a rigid flex that has a BGA-113 (microstar BGA) package to be mounted to it. The routing in this area on the top layer leaves me with .0005 of soldermask clearance from the edge of the BGA pad and .003 distance from the edge of the soldermask to the nearest track- in other words I have .0035 of clearance from pad edge to next track assuming a perfect etch and perfect soldermask registration. Having rooted around Texas Instruments web site I believe that it may be possible to reflow this BGA without adding solder paste to the pad - just letting the ball collapse do the attachment. If my scenario is correct I could open up the soldermask and not have too many concerns about bridging between the BGA pads and the tracks. Any thoughts or comments would be appreciated. Thanks Steve Kelly Steve Kelly (PLEASE NOTE NEW E-MAIL ADDRESS) (416) 750-8433 (work) (416) 750-0016 (fax) (416) 577-8433 (cell) --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------