Hi Bill, What might be happening is that the layer of HASL is too thin and almost all Sn is consumed to form intermetallics. You wouldn't see any contamination on the surface, but would have trouble soldering to it, unless a fresh surface is exposed (the surface is scrubbed). I would be able to confirm that if I had a sample. Regards, Vladimir SENTEC SENTEC 11 Canadian Road, Unit 7. Scarborough, ON M1R 5G1 Tel: (416) 899-1882 Fax: (905) 882-8812 www.sentec.ca -----Original Message----- From: Bev Christian <[log in to unmask]> Date: Mon, 15 Jun 2009 14:27:39 To: <[log in to unmask]> Subject: Re: [TN] Fw: [TN] HAL-Leaded assembly Bill, No prob. I should have been able to figure that out. I'm just used to seeing HASL. Bev -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Bill Dworak Sent: Monday, June 15, 2009 2:16 PM To: [log in to unmask] Subject: [TN] Fw: [TN] HAL-Leaded assembly Sorry Bev, I am guilty of using terminology that is specific to my end of the industry. Hot air leveling (HAL) leaded, means that the surface finish is tin lead , I defined it as leaded because there is a leaded as well as non-leaded surface finish out there now. This is a military account so we cannot use no-lead. I did leave out the materials used typically it has been FR4, 130 as well as 170. Sorry. Bill ----- Original Message ----- From: "Bev Christian" <[log in to unmask]> To: <[log in to unmask]>; <[log in to unmask]> Sent: Monday, June 15, 2009 10:53 AM Subject: Re: [TN] HAL-Leaded assembly Bill, Not enough info! What surface finish? What board type? What environment boards stored in? How long between manufacture of boards and use? Bev RIM ----- Original Message ----- From: TechNet <[log in to unmask]> To: [log in to unmask] <[log in to unmask]> Sent: Mon Jun 15 13:47:51 2009 Subject: [TN] HAL-Leaded assembly Hello everybody, I am looking for some knowledge on what I see is a basic type problem that is driving me crazy. I am a sales guy who covers a sizable territory and in that territory for a PCB manufacturer (yes one of those) I have one account that I have been working with for about 4 years now that continuously has issues assembling both hand assembly as well as pick & place. The surface finish is HAL (leaded) this is a military account that is pretty well structured in their processes. What I get told is that there seems like a contamination is on the surface when they scrub the surface it makes it better but not 100% better.They have sent back samples for us to look at , we saw nothing on the surface no contamination nothing wrong at all. If this was one of a few that has the same or similar issues it would make some sense and I could go to the people I work with asking them to look into this issue. But it is the only company that has this issue. Has anybody seen a similar type of a situation before? Understood that you cannot fix this but would appreciate advise as to where to look so hopefully this can be solved. Thank you. Bill Dworak --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------------------------- This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful. --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------