Hi Rob, No 'baking ' benefit is likely from baking above Tg; however, I am really concerned about solderability as well as damage to the PCB resin, sitting this long above Tg with its large CTE. Werner -----Original Message----- From: Rob Strecker <[log in to unmask]> To: [log in to unmask] Sent: Mon, 4 May 2009 10:54 am Subject: Re: [TN] PCB baking I have read the same thing. 105 - 125C around 4 hours. Our PCB supplier has had issues with the pressing time in there process and we are seeing more delamination on our boards again. They have recommended we bake our existing stock, 5 boards stacked in the oven, at 180C for 2 hours (including ramp). My main concern is the solderability of the ENIG finish after this baking profile. They have shown me some pictures after bake and the gold is darkening. They are asking us if this is acceptable because the boards passed a solder dip test. We are going to bake some boards ourselves, paste and reflow to see the impact. Any thoughts on the 180C bake temp? It seem as though they want the bake temperature above the Tg temp (170) not sure why? Rob Strecker -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /* Sent: Monday, May 04, 2009 7:57 AM To: [log in to unmask] Subject: Re: [TN] PCB baking Hi Ioan, No there is not, and there really cannot be. The temperatures used are in the range of 105 to 125-I tend towards 10 5 C, but the duration depends on a whole lot of factors. Among them: moisture content [bake time ranging from 0 to 24 hours plus], construction [thickness, P/G layer location, PCB resin, resin content, PTH/via pitch/diameter], reflow process/temperature, etc. My recommendation is to determine it yourself on some coupons supplied with the PCBs. Werner -----Original Message----- From: Ioan Tempea <[log in to unmask]> To: [log in to unmask] Sent: Mon, 4 May 2009 9:25 am Subject: [TN] PCB baking Dear Technos, I know this has been oftenly discussed here, but I would like to lively up the traffic a little bit... Is there any IPC standard reglementing the bake out time for PCBs, in terms of temperature/dwell time? Thanks, Ioan Tempea, ing. Ingénieur Principal Fabrication / Sr. Manufacturing Engineer 30 ans déjà! - Already 30 years! 950 rue Bergar, Laval, Québec, H7L 5A1 t : 450-967-7100 ext : 244 Mtl : 514-990-5762 f : 450-967-7444 [log in to unmask] <mailto:[log in to unmask]> www.digico.cc <http://www.digico.cc/> P N'imprimer que si nécessaire - Print only if you must --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]:20SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------