Inge: Technically speaking there is a large difference between a wax and a polish. A polish does grind down the surface, and may or may not leave a coating behind. A wax is primarily a coating, and often does little if any "grinding down" of the surface. The thickness of any coating left by either wax or polish is going to be a function of not only composition of the wax/polish, but also how aggressive the mechanical polishing is. Some polishes leave only a mono-molecular film of anti-tarnish. Rudy Sedlak RD Chemical Company --- On Fri, 5/29/09, Victor Hernandez <[log in to unmask]> wrote: From: Victor Hernandez <[log in to unmask]> Subject: Re: [TN] WAX To: [log in to unmask] Date: Friday, May 29, 2009, 8:24 AM A picture is worth a thousand words. -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Sent: Friday, May 29, 2009 9:34 AM To: [log in to unmask] Subject: [TN] WAX Hi all and even Bev, Assume that you polish a metal, in my case five 9s Ag. Polishes have at least two purposes. Grind the metal to get a certain level of brightness (we polish to Ra 30 nanometers). And leave a thin coating that protects the metal. Now, in our case, what is left is so thin, that you can't observe the 'coating'. Presumably because it's an organic compound of some sort, and also because it's transparent for our eye's wavelength. Now comes the question: has anyone out there ever investigated such a 'wax' and determined the thickness, and if so, what kind of equipment was used? That's why I more or less directed the q to Bev... Inge --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------