Electrostatic fields can be induced in high dielectrics and once there, may be hard to get rid of. As little as 50 VDC can be a problem for IC chips without enough I/O diode protections. We have had some issues which might have been caused by such surface charges, but we could never prove it. To be sure , we demand ESD safe bags. Additional cost negligible. Inge ----- Original Message ----- From: "John Parsons" <[log in to unmask]> To: <[log in to unmask]> Sent: Thursday, May 14, 2009 8:36 PM Subject: [TN] Bare PCB Packaging Requirements > Tell us, how many CEM's out there are demanding that bare PCB's be > received > in vacuum sealed moisture barrier anti-static bags. If so, what is your > reasoning? Just to be clear my focus here is "anti-static" not the > moisture > barrier properties of the packaging. > > > > Regards > > > > John Parsons > > > > > --------------------------------------------------- > Technet Mail List provided as a service by IPC using LISTSERV 15.0 > To unsubscribe, send a message to [log in to unmask] with following text in > the BODY (NOT the subject field): SIGNOFF Technet > To temporarily halt or (re-start) delivery of Technet send e-mail to > [log in to unmask]: SET Technet NOMAIL or (MAIL) > To receive ONE mailing per day of all the posts: send e-mail to > [log in to unmask]: SET Technet Digest > Search the archives of previous posts at: http://listserv.ipc.org/archives > Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 > for additional information, or contact Keach Sasamori at [log in to unmask] or > 847-615-7100 ext.2815 > ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------