Genny, The bottom line is that if moisture is absorbed into the connector material and is reflowed without drying the part will "Popcorn", as someone had earlier mentioned. Doug Erb ダグ・アブ Senior FAE Hirose USA -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard Sent: Wednesday, May 13, 2009 1:23 PM To: [log in to unmask] Subject: Re: [TN] Nylon connectors - moisture sensitivity This is a shrouded header, 2mm spacing on the pins. Basic. Nothing high frequency. It is surface mount, it is designed for reflow. This one is specified that it can withstand one reflow of 260C for 10 seconds. When this connector arrived, it was in MBB packaging. When we asked about that, we were told, 'treat it as equivalent to 5a MSL'. This is the first time I have ever heard of a basic connector being MSL. We received it on tape and reel. However, we were told that if it is out of MBB for longer than 24 hours that we should bake at 120C for 4 hours. We will have to take it out of T&R to do that, which means it would need to be repackaged. I should clarify - when I talked about melting connectors I was talking in general terms, not this specific connector. I'm sure we've all melted a connector from time to time. I was trying to understand what would happen, what kind of damage would we see, if it was moisture-laden and we reflowed it anyway? Genny -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge Sent: May 13, 2009 1:22 PM To: [log in to unmask] Subject: Re: [TN] Nylon connectors - moisture sensitivity Genny, first of all, you should ask yourself : - what is the system impedance (50 Ohm or MOhms) - signal levels - current levels - DC? - AC? - data lines? - wave form? - S/N requirements?¨ - Insulation requirements (flashover risk) - pin/sleeve basic metal? - ditto plating? - migration condtions? - nylon reinforcement? Then you can judge the situation and decide what level of risk. In certain situations not even Teflon is satisfactory. Inge ----- Original Message ----- From: "Genny Gibbard" <[log in to unmask]> To: <[log in to unmask]> Sent: Wednesday, May 13, 2009 8:43 PM Subject: [TN] Nylon connectors - moisture sensitivity We have been told that a surface mount nylon connector we use is moisture sensitive, and should be treated as equivalent to level 5a. This is the highest level we have ever seen on any component we have used of any type. I didn't think that a connector could be moisture sensitive. Not heat tolerant, yes - we have melted a few - but moisture sensitive? What kind of damage can happen to a nylon connector from too much moisture absorption? Thanks in advance for your responses. Genny --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------