Whenever I am asked what finish I would choose if I had to choose only one and it had to work for everything and I still wanted to be able to sleep at night: ENEPIG is my answer. Just like my vintage humor, whatever I say I always want to come up with the best finish. Dewey -----Original Message----- From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Whiteman Sent: Thursday, April 23, 2009 11:11 AM To: [log in to unmask] Subject: [TN] Electroless Nickel Electroless Palladium Immersion Gold (ENEPIG) Does anyone have any opinions of using Electroless Nickel Electroless Palladium Immersion Gold (ENEPIG) as a board finish for high reliability aerospace applications? You can contact me off line if necessary... Thanks again. Lee Whiteman, PMP Senior Member Engineering Staff L-3 Communications East Telephone: (856) 338-3508 FAX: (856) 338-2906 E-Mail: [log in to unmask] --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 ----------------------------------------------------- --------------------------------------------------- Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 -----------------------------------------------------